액화 헬륨 조건에서 극저온 접착제 Lap shear strength test 시 기계물성 변화 및 실험 개선에 대한 연구 Research for Change of Mechanical Properties of Cryogenic Adhesive with Lap Shear Strength Test in Liquified Helium Condition and Improvement of Test

표창민, 김성환, 김재웅
  • 언어KOR
  • URLhttp://db.koreascholar.com/Article/Detail/412722
한국기계기술학회지 (韓國機械技術學會誌)
제24권 제1호 (2022.02)
pp.78-84
한국기계기술학회 (Korean Society of Mechanical Technology)
초록

Conversion to modern hydrogen energy is required, and research on liquefied hydrogen cargo containment systems is needed for large-capacity transport and storage. In this study, changes in the mechanical properties of the adhesive required for storage and transport in liquid hydrogen were confirmed. The lap shear test was performed by realizing cryogenic conditions in a small chamber using liquid nitrogen and liquid helium. There was an increase of 11.0% in the -180℃ condition compared to room temperature, and an increase of 1.8% in the -230℃ condition compared to the -180℃ condition was confirmed. In the case of shear strain, it is known that it decreases as the temperature goes down. As a result of the experiment, it was confirmed that the value at room temperature and the value at -180℃ reduced the shear strain by 5.0%, and -230˚ compared to the -180℃ condition. An increase of 1.5% was confirmed in the C condition. In the case of the specimen tested at -230℃, the deformation in the gripper part was larger than in other tests, and it is judged that the maximum shear strength and shear strain were affected. In addition, in this study, there is a limitation in the experiment at -230°C rather than 253°C, which is the boiling point of hydrogen

저자
  • 표창민(한국생산기술연구원) | Chang-Min Pyo
  • 김성환(한국생산기술연구원) | Kim Sung-hwan
  • 김재웅(한국생산기술연구원) | Jaewoong Kim