논문 상세보기

습식환원법에서 NaBH4환원제를 이용한 Ag분말의 제조 KCI 등재

Preparation of Ag Powder by Wet Reduction Method using NaBH4 Reducing Agent

  • 언어KOR
  • URLhttps://db.koreascholar.com/Article/Detail/2489
구독 기관 인증 시 무료 이용이 가능합니다. 4,000원
한국분말야금학회지 (Journal of Korean Powder Metallurgy Institute)
한국분말재료학회(구 한국분말야금학회) (Korean Powder Metallurgy Institute)
초록

Spherical Ag powder was prepared in the system of by wet chemical reduction method. The size of Ag powder was increased as the reaction temperature and the concentration of reducing agent was decreased in the constant concentration of dispersion agent. Optimum conditions of producing Ag powder having of D50 was 1M of , 0.5M of , 1.5g of Gelatine in the room temperature.

저자
  • 원창환 | Won Chang-Whan
  • 이혁희 | Lee Huk-Hee