To developed new process for obtaining maximum molecular weight of anionic acrylamide and acrylic acid copolymer by inverse emulsion polymerization. Concentration of initiator, reducing agent, surfactant and mole ratio of acrylamide-acrylic acid were studied for the process. Semi-batch processes with method of redox, control of reaction temperature, feeding method of monomer and reaction time, was suitable for maximum molecular weight of P(AMAC) from this process obtained 3.09 × 106(Mn.) and 4.41 × 106(Mw.) in molecular weight measured by the intrinsic viscosity method. inverse emulsion polymerization mechanism of P(AMAC) does not followed the Smith-Ewart and Medvedev theory, but selected for concentration of initiator, reducing agent, surfactant, water solubility of monomer.