In the preparation of acrylic water repellent(EDLWC). quaternized 2-diethylarrunoethylmethacrylate-stearylmethacrylate copolymer (DSACC) and quaternized 1-Iaurovlbis(aminoethyl)-2-dodecylimidazoline(LDDIC) were selected as a basic resin and the improving agent such as softening effect and hydrostatic pressure of the water repellent. EDLWC was prepared by blending waxes and emulsifier for waxes with various ratio to DSACC and LDDIC. As the results of the measurement of water repellency, washable, tear strength and crease recovery to polyester-cotton(P/C) blended fabrics treated with EDLWC only or addition of textile finishing resin, the physical properties were increased. Sodium acetate was the most effective catalyst in the water repellency among the various kinds of catalyst. and the reasonable concentration of the catalyst was 1. 4 wt%. EDLWC was confirmed as durable water repellent with the results of making little difference of water repellency as ±5 point after and before washing. The reaction mechanism between P/C blended fabrics and EDLWC in the presence of catalyst was proposed. And also, the longitudinal view of the P/C blended fabrics treated with water repellent was observed with scanning electron microscope.