The Cuo-Magnetite and ZnO-Magnetite catalysts with various of Cuo and ZnO mole% for Carbon Dioxide decomposed reaction synthesized. The catalysts were reduced by H2 at 350℃ for 3 hours. The temperature was obtained by TGA and DSC experiments. The structures of catalysts were confirmed by X-ray diffraction experiment. The surface area of catalysts is 15~27 m2/g. The results of Carbon Dioxide decomposed ability was better H2-reduced magnetite catalysts with 0.03 mole% CuO and 0.03 mole% ZnO than others catalysts. After Carbon Dioxide decomposed reaction, catalysts were reacted H2 and created only methane.