The p-type thermoelectric compounds of based doped with 3wt% Te were fabricated by a combination of rapid solidification and spark plasma sintering (SPS) process. The effect of holding time during spark plasma sintering (SPS) on the microstructure and thermoelectric properties were investigated using scanning electron microscope (SEM), X-ray diffraction (XRD) and thermoelectric properties. The powders as solidified consisted of homogeneous thermoelectric phases. The thermoelectric figure of merit measured to be maximum () at the SPS temperature of .

저자
  • 문철동 | Moon Chul-Dong
  • 홍순직 | Hong Soon-Jik
  • 김도향 | Kim Do-Hyang
  • 김택수 | Kim Taek-Soo)