To the goal of improving the early compressive strength of the mortar including Ground granulated
blast furnace slag under low-temperature environment, Industrial byproducts including SiO2 and Al2O3 was fired and than 7% of it was added into Ground granulated blast furnace slag. By checking compressive strength and activity index from different mixing rate, in spite of low strength development than OPC 100%, when using firing powder, the expectation of increasing strength by curing time was affirmative