고성능 그라우트를 사용한 풍력타워 연결부의 부착거동에 대한 실험적 연구

An experimental study on the bond characteristic of transition piece of wind turbine tower using high performance grout

  • 언어KOR
  • URLhttps://db.koreascholar.com/Article/Detail/293556
서비스가 종료되어 열람이 제한될 수 있습니다.
한국구조물진단유지관리공학회 (The Korea Institute For Structural Maintenance and Inspection)
초록

In this study, bond performance of grouted joint with high performance cement grout was verified. The grout which the compressive strength of grout was over 120MPa. was applied for wind turbine tower connections. From the results, the connection joint using high performance grout has sufficient bond strength.