To evaluate the durability characteristics of low permeable concrete using ground granulated blast-furnace slag with fineness 4,650 cm2/g, carbonation depth was measured. From the test results, persisting period of that was calculated. And it was found that carbonation depth of concrete was proceed 29.5 mm for 100 years.