방전플라즈마소결법을 이용한 WC-3 wt%Co 소결체 제조 및 평가 KCI 등재 SCOPUS

Fabrication and Evaluation of WC-3 wt%Co Compacts Fabricated by Spark Plasma Sintering

  • 언어KOR
  • URLhttps://db.koreascholar.com/Article/Detail/296863
구독 기관 인증 시 무료 이용이 가능합니다. 4,000원
한국재료학회지 (Korean Journal of Materials Research)
한국재료학회 (Materials Research Society Of Korea)
초록

Microstructure and mechanical properties of WC-3wt% Co cemented carbides, fabricated by a sparkplasma sintering (SPS) process, were investigated in this study. The WC-3wt%Co powders were sintered at900~1100oC for 5min under 40MPa in high vacuum. The density and hardness were increased as the sinteringtemperature increased. WC-3wt%Co compacts with a relative density of 97.1% were successfully fabricated at1100oC. The fracture toughness and hardness of a compact sintered at 1100oC were 21.6MPa·m1/2 and4279Hv, respectively.