For the CLMS using FA as powder and S and SS as fine aggregates, respectively, in order to improve flowability by preventing material separation and securing quantity of minimum unit and to secure maximum strength by repressing bleeding, the most reasonable and optimal combinations of FA+S and FA+SS were f/a 20 and f/a 60, respectively.