Accelerated alkali resistance test were conducted for pre-heated GFRP Rebar. The GFRP rebar specimens were heated to temperatures of 60℃, 120℃, 200℃ and 300℃ and then immerged in alkali solution for 30days. According to ACI 440.3R-12, tensile properties were measured.