In this paper, the recovery stress of Fe based Shape Memory Alloy(Fe-SMA) was investigated. The temperature of the Fe-SMA was heated to 160℃ and then cooled to evaluate the recovery stress. Pre-strain 2% and 4% was considered as experimental variables. The recovery stress of pre-strain 2% and 4% are 358MPa and 397MPa, respectively.