        43.
        2002.06 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김병기, 김진천, 하국현, 최철진
        Nanosized tungsten carbide powders were synthesized by the chemical vapor condensation(CVC) process using the pyrolysis of tungsten hexacarbonyl(). The effect of CVC parameters on the formation and the microstructural change of as-prepared powders were studied by XRD, BET and TEM. The loosely agglomerated nanosized tungsten-carbide() particles having the smooth rounded tetragonal shape could be obtained below in argon and air atmosphere respectively. The grain size of powders was decreased from 53 nm to 28 nm with increasing reaction temperature. The increase of particle size with reaction temperature represented that the condensation of precursor vapor dominated the powder formation in CVC reactor. The powder prepared at was consisted of the pure W and cubic tungsten-carbide (), and their surfaces had irregular shape because the pure W was formed on the powders. The and W powders having the average particles size of about 5 nm were produced in vacuum.
        4,000원
        45.
        1999.03 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천, 김종수, 조정식, 최기석, 이광래
        폴리설폰 중공사막에 대한 산소와 질소의 투과도에 미치는 수분의 영향에 대한 실험을 수행하였다. 상대습도가 증가할수록 수분을 함유한 산소와 질소의 투과도는 감소하였따. 공급압력 3 kgf/cm2와 온도 30℃에서, 상대습도 100% 인 산소의 투과도는 건조산소의 투과도보다 20%만큼 감소하였으며, 질소는 14%만틈 감소하였다. 수분을 gkadmb한 산소의 투과도는 운전시간이 경과함에 따라 단조하게 감소하여 정상상태에 도달하였다. 그러나, 질소의 투과도는 일시적으로 증가하였다가 감소하여 정상상태에 도달하였다.
        4,000원
        46.
        1998.09 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천
        The W-Cu composite powders were synthesized from W and Cu elemental powders by ball-milling process, and their microstructural changes and sintering behaviors were evaluated. The ball milling process was carried out in a 3-dimensional mixer (Turbula mixer) using zirconic () ball and alumina () vial up to 300 hrs. The ball-milled W-Cu powders revealed nearly spherical shape. Microstructure of the composite powders showed onion-like structure which consists of W and Cu shells due to the moving characteristic of Turbula mixer. The W and Cu elements in the composite powders milled for 300 hrs were homogeneously distributed, and W grain size in the ball-milled powder was smaller than 0.5 . Fe impurity introduced during ball milling process was very low as of 0.001 wt%. The relative sintered density of ball-milled W-Cu specimens reached about 94% after sintering at .
        4,000원
        50.
        1998.06 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천
        W-Cu alloy is attractive to thermal managing materials in microelectronic devices because of its good thermal properties. The metal injection molding (MIM) of W-Cu systems can satisfy the need for mass production of the complex shaped W-Cu parts in semiconductor devices. In this study, the application of MIM process of the mechanically alloyed (MA) W-Cu composite powders, which had higher sinterability were investigated. The MA W-Cu powders and reduction treated (RT) powders were injected by using of the multicomponent binder system. The multi-stage debinding cycles were adopted in and atmosphere. The isostatic repressing treatment was carried out in order to improve the relative density of brown parts. The brown part of RT W-Cu composite powder sintered at 110 had shown the higher sinterability compared to that of MA powder. The relative sintered density of all specimens increased to 96% by sintering at 120 for 1 hour. The relationship between green density and the sintering behavior of MA W-Cu composite powder was analyzed and discussed on the basis of the nanostructured characteristics of the MA W-Cu composite powder.
        4,000원
        51.
        1998.06 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천
        Sintering behavior of nanostructured(NS) W-Cu powders prepared by mechanical alloying (MA) was investigated as a function of sintering temperature. MA NS W-2owt%Cu and W-3owt%Cu composite powders with the crystal size of 20-30 nm were annealed at 90, and thermal characteristics of those powders were investigated by DSC. Sintering behavior of MA NS W-Cu composite powders was investigated during the solid-state sintering and the Cu-liquid phase sintering. The new nanosintering phenonenon of MA W-Cu powders at solid-state sintering temperature was suggested to explain the W-grain growth in the inside of MA powders. The sintering densification of MA NS W-Cu powders was enhanced at Cu melting temperature by arrangement of MA powders, i.e., the first rearrangement of MA powders was occurred, and then the rearrangement of W-grains in the sintered parts was also took place during liquid-phase sintering, i.e., the second rearrangement was happened. Due to the double rearrangement process of MA NS W-Cu powders, the high sintered density with more than 96%o was obtained and the fine and high homogeneous state of W and Cu phases was achieved by sintering at 1200 .
        4,000원
        55.
        1997.06 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천
        Nanostructured(NS) W-Cu composite powders of about 20~30 nm grain size were synthesized by mechanical alloying. The properties of NS W-Cu powder and its sintering behavior were investigated. It was shown from X-ray diffraction and TEM analysis that the supersaturated solid solution of Cu in W was not formed by the mechanical alloying of mixed elemental powders, but the mixture of W and Cu particles with nanosize grains, i.e., the nanocomposite powder was attained. Nanocomposite W-20wt%Cu and W-30wt%Cu powders milled for 100 h were sintered to the relative density more than 96% and 98%, respectively, by sintering at 110 for 1 h in . Such a high sinterability was attributed to the high homogeneous mixing and ultra-fine structure of W and Cu phases as well as activated sintering effect by impurity metal introduced during milling.
        4,200원
        58.
        1996.03 KCI 등재 구독 인증기관 무료, 개인회원 유료
        김진천
        Nanostructured Cu-Pb powders were synthesized by mechanical alloying process. The variation of powder characteristics with mechanical alloying time was investigated by x-ray diffraction, differential scanning calorimetry, SEM and TEM. An electrical resistivity of the hot pressed specimens was also measured by using the nanovoltmeter. It was shown that mechanical alloying for 12 hours leads to a homogenization and a grain refinement to the nanometer scale under 20 nm. The mechanically alloyed Cu-Pb alloys represented the enhanced solid solubility of 10wt% Pb in the Cu matrix. The monotectic temperature of nanostructured Cu-Pb alloy decreased from equilibrium state of 955 to 855 due to reduced grain size effect. The analysis of electrical resistivity showed that the hot pressed MA Cu-5wt% Pb compact existed as a solid solution.
        4,000원