        PURPOSES : The use of hydrated lime or other liquid anti-stripping agents (ASA) is the most common method of improving the moisture susceptibility of asphalt mixes. ASAs are also known to have an anti-aging effect, according to several researchers. Therefore, the use of ASAs is expected to enhance the stability of asphalt pavements. The purpose of this study is to investigate the anti-aging effect of ASAs that are found in the domestic market. METHODS : In this study, an asphalt binder and a mixture mixed with typical domestic solid and liquid ASAs were prepared and aged to evaluate the physicochemical changes. A liquid additive developed by a Korean oil refinery was used as the liquid ASA, and hydrated lime was utilized as the solid ASA. The aging process of the asphalt was determined in the laboratroy based on previous studies to simulate the aging process inh te field. RESULTS : The result of the laboratory experiment indicates that both the solid and liquid ASAs have an anti-aging effect. Moreover, the liquid additive performed relatively better than the hydrated lime. CONCLUSIONS : If ASAs have an anti-aging effect in addition to the anti-stripping function, it is expected to improve the stability of the asphalt pavement significantly. However, few studies have been carried out on the anti-aging effect of ASAs found in the domestic market. In this study, we conducted a fundamental study on the anti-aging effect to help in the selection and use of ASAs in the domestic asphalt-paving industry.
        4,000원
        3.
        2015.10 구독 인증기관·개인회원 무료
        아스팔트 콘크리트 포장 포토홀은 최근 차량 파손등 운전자의 쾌적한 주행에 악영향을 주고 있다. 포토 홀은 아스팔트 콘크리트 포장의 수분민감저항성이 떨어져 발생하는 파손형태로 국토교통부에서 아스팔트 혼합물의 간정인장강도비를 80% 상향 조정하였으며 80%에 미달하는 아스팔트 혼합물은 박리방지제를 사 용하도록 규정하고 있다. 본 연구에서는 아스팔트 혼합물의 수분민감 저항성을 증가시키기 위하여 박리방지제 사용하였으며, 초 기 박리방지제의 성능검증을 판별하기 위해 보일링(Boiling Water Test, ASTM D 3625-96) 시험을 실 시 하였다. 간접인장강도 시험은 시편을 7.0±0.5% 공극률로 제작하였으며, 습윤(동결융해), 건조 샘플을 나누어 실험을 진행하였고 간접인장강도(Indirect Tensile Strength)를 측정하여 간접인장강도비 (Tensile Strength Ratio)를 산정하였다. 간접인장강도 시험 분석결과 습윤시편과 건조시편의 강도 차이가 무첨가 아스팔트 혼합물에서는 차이 가 분명하게 나타났지만, 액상박리방지제 첨가 시편들에서는 근소하게 나타났다. 간접인장강도비 분석결 과 액상박리방지제 무첨가 시편은 53%, 개발한 액상방리방지제 첨가 시편은 기준치인 80% 이상으로 나 타나 미국의 상용 박리방지재와 별 차이가 없었다.