This study presents the results of experimental research to investigate the drying shrinkage properties of mortar containing the fly-ash and glycol-ether shrinkage reducing agent. the drying shrinkage of mortar was measured according to KS F 2424. It was confirmed from test results that 10% fly-ash replacement and 1% shrinkage reducing agent is most effective to decrease the shrinkage of mortar
This study presents the results of experimental research to investigate the drying shrinkage properties of mortar containing the fly-ash and glycol-ether shrinkage reducing agent. the drying shrinkage of mortar was measured according to KS F 2424. It was confirmed from test results that 10% fly-ash replacement and 1% shrinkage reducing agent is most effective to decrease the shrinkage of mortar.