        2015.08 KCI 등재 SCOPUS 구독 인증기관 무료, 개인회원 유료
        In this study, low-carbon hypoeutectoid steels with different ferrite-pearlite microstructures were fabricated byvarying transformation temperature. The microstructural factors such as pearlite fraction and interlamellar spacing, and cementitethickness were quantitatively measured and then Charpy impact tests conducted on the specimens in order to investigate thecorrelation of the microstructural factors with impact toughness and ductile-brittle transition temperature. The microstructuralanalysis results showed that the pearlite interlamellar spacing and cementite thickness decreases while the pearlite fractionincreases as the transformation temperature decreases. Although the specimens with higher pearlite fractions have low absorbedenergy, on the other hand, the absorbed energy is higher in room temperature than in low temperature. The upper-shelf energyslightly increases with decreasing the pearlite interlamellar spacing. However, the ductile-brittle transition temperature is hardlyaffected by the pearlite interlamellar spacing because there is an optimum interlamellar spacing dependent on lamellar ferriteand cementite thickness and because the increase in pearlite fraction and the decrease in interlamellar spacing with decreasingtransformation temperature have a contradictory role on absorbed energy.
        4,000원