        This study was conducted to prepare acrylic removable protective coatings by emulsion polymerization. Monomers used were n-butyl acrylate, acrylonitrile, butyl methacrylate. Emulsifiers used were sodium lauryl sulfate and polyoxyethylene lauryl ether, which are an anionic emulsifier and a nonionic emulsifier respectively. Potassium persulfate was used as an initiator and polyvinyl alcohol was used as a stabilizer. Emulsion polymerization was carried out in a semi-batch reactor at 70℃ and agitation speed was 200 rpm. Tensile strength, extension, peel strength, viscosity, and solid contents of the synthesized coatings were examined. The coatings prepared with BA:AN = 60:20 (in weight ratio) satisfied the standard for automobile in terms of extension and peel strength. When the concentration of BMA was in a range of 18~23 wt%, the prepared coatings satisfied the standard for automobile in terms of peel strength and water resistance.