환경친화성 하이솔리드 도료의 제조 및 고형분 함량에 따른 도막물성 변화 KCI 등재

Preparation of Environmental Friendly High-Solid Coatings and Their Property Changes with Solid Contents

  • 언어KOR
  • URLhttps://db.koreascholar.com/Article/Detail/257502
구독 기관 인증 시 무료 이용이 가능합니다. 4,000원
한국응용과학기술학회지 (The Korean Society of Applied Science and Technology)
한국응용과학기술학회(구 한국유화학회) (The Korean Society of Applied Science and Technology (KSAST))
초록

Room temperature cure type of acryl-urethane coatings with high solid content were prepared in this study. Acrylic resins with 80% solid content were cured with hexamethylene diisocyanate (Desmodure N-3600). The cure time of prepared coatings BEHCC-84 (BEHC-84 : Tg=0℃) and BEHCC-87 (BEHC-87 : Tg=30℃), measured by rigid-body pendulum method, was recorded 8.3 hours and 3.8 hours, respectively. Dynamic viscoelastic experiment also revealed the glass transition temperature of BEHCC-84 and BEHCC-87 to be Tg=40.3℃ and Tg=43.3℃, respectively. It was found that the adhesion and flexural properties among various propeties of coatings were enhanced by the incorporation of caprolactone acrylate monomer into the acrylic resins.

저자
  • 박홍수 | Park, Hong-Soo
  • 조혜진 | Jo, Hye-Jin
  • 심일우 | Shim, Il-Woo
  • 유혁제 | You, Hyuk-Jae
  • 김영찬 | Kim, Young-Chan