The components of municipal solid waste incineration bottom ash produced over 3 million ton every year are similarto the components of geological features, therefore it is suitable to be used as the raw materials of lightweight aggregate.Development of lightweight aggregate using this bottom ash will be helpful to solve landfill and environmental problems.Lightweight aggregate was developed at 1,110oC by using clay, kaolin, bentonite and silica as the raw material to 50%of municipal solid waste incineration bottom ash. Silicon carbide (SiC) was used as a blowing agent. Optimal mixingratio is bottom ash 50%, kaolin 22%, clay 22%, bentonite 6% and blowing agent 0.1%. As the result of quality test,produced lightweight aggregate met the all appraisal standards. The result of heavy metal leaching test was much lowerthan the elution reference value of ceramic manufactures made by using bottom ash.