In this study, high-ductile and low-fiber composites have been mixed using Alkali-activated cement-free binders combined with PVA fibers of the volume fraction of 1.0~1.5%. From the direct tensile test of the composites, the low-fiber cement-free composites could exhibit high-ductile tensile behaviors about 4.0~7.0% tensile strains after cracks.