The effect of different cooling rate on the structure and mechanical properties of Fe-3%Mn-(Cr)-(Mo)-0.3%C steels is described. Pre-alloyed Astaloy CrM and CrL, ferromanganese and graphite were used as the starting powders. Following pressing in a rigid die, compacts were sintered at and in atmospheres and cooled with cooling rates and . Convective cooled specimens were subsequently tempered at for 60 and 240 minutes.