Experimental results show that the maximum temperature of the floorboard surface is 1/2 level compared to the hot water temperature of 80℃, which is circulated by hot water heating. And the part above 10mm above the surface of the floorboard was low as 1/3 level. Therefore, in order to improve the heating efficiency of the room where the flooring is applied to the hot water heating, the thermal conductivity of the flooring material should be improved as well.
The purpose of this study is to investigate the mechanical property of concretes using surface treated lightweight aggregate. Slump of concretes using surface treated lightweight aggregate measured 120~140mm, which are lower than slump of NWAC. Compared to compressive strength of NWAC, compressive strength of concretes using surface treated lightweight aggregate showed a level of 82.8~95.9%.