        Two kinds of Bi2Te3 powders, pure Bi2Te3/2vol.%ZrO2, have been prepared by a mechanical grinding process process. Effect of mixing of the powders on thermoelectric of the sintered body has been investigated by measuring Seebeck Coeffcient, specific electric resistivity and thermal conductivity. With an increase in the weight fraction of the Bi2Te3/2vol.%ZrO2 powder from 0 to 40wt.%. Especially, the figure of merit of the mixedBi2Te3 sintered body increases and thereafter dedreases above 40wt.%. Especially. the figure of merit of the mixed Bi2Te3 sintered bodies with mixing of Bi2Te3/2vol.%ZrO2 powder increased about 1.3time in comparison with the value of the specimen before mixing. Mixing of two kinds of Bi2Te3 powders which have different theramal and electric propertries with each other seemed to be useful methob to increase the figure of merit of Bi2Te3 sintered body.