In this study, high strength concrete with satuated artificial lightweight aggregate(SLWA) produced by domestic for reducing autogenous shrinkage, which provides additional water to the hydratin cement particles, is applied to be the internal curing. This paper presents the test result of basic property of SLWA and autogenous shrinkage with volumes of SLWA.