        One disadvantage of deep cycle flooded lead-acid batteries is increasing water loss caused by use of (+) Pb-Sb / () Pb-Sb alloy grid. Water loss is generated by the emission of hydrogen gas from the () electrode during battery charging. In this paper, we maintain cycle life aspect through the development of hybrid flooded lead-acid batteries to which a (+) Pb- Sb / () Pb-Ca grid is applied and deal with the improvement of water loss. The amount of water loss compared to that of the () Pb-Sb grid decreased when Ca was added to the () Pb grid. For the () Pb-Ca grid, it was confirmed that the time to reach 0.0 V, at which water decomposition occurs, was increased compared to that of the () Pb-Sb grid at the NPV (Negative Potential Voltage). In the cycle life test conducted with the BCI (Battery Council International) standard, compared to the (+) Pb-Ca grid, the (+) Pb-Sb grid increased the life cycle of the batteries and the (+) Pb-Ca grid showed an early end of life due to PbO corrosion layer generation, as determined through SEM / EDS and Tear Down analysis. In conclusion, by addition of Sb to (+) Pb grid and Ca to () Pb grid, we developed a hybrid flooded lead-acid battery that meets user requirements to improve water loss characteristics and preserve cycle life characteristics.
        4,000원