        Porous poly(e-caprolactone) (PCL) scaffolds were fabricated by salt leaching method. The PCL scaffolds were treated with aqueous NaOH for 0h, 2h, 4h, 8h, and 12h at 40˚C. The NaOH-treated PCL scaffolds were dipped in CaCl2 and K2HPO4·3H2O solution alternately three times to induce apatite nuclei onto the surface of the scaffolds. The NaOH-treated PCL scaffolds were immersed into SBF solution for 1day to grow the apatite. The apatite formation were investigated as a fuction of NaOH treatment time. The hydrophilicty and surface area of the PCL scaffolds were increased with NaOH-treatment time. The NaOH-treated PCL scaffolds were successfully formed a dense and uniform bone-like apatite layer after immersion for 1 day in SBF solution.