In this study, it was developed geopolymer concrete of alkali-activated using the mixed fly ash and blast furnace slag. and it was developed the interlocking block using the developed geopolymer concrete. In addition, the bending strength and water absorption rate of the interlocking block was tested by KS standard. The test results were as follows. The water adsorption ratio of the BSF4 specimen was under 10%, and the flexural strength of that was over 5MPa