        검색결과 4

        1.
        2017.04 서비스 종료(열람 제한)
        This study was conducted to examine the workability of LEFC in relation to the types and the mix ratio of different foaming agents. The foam agents act as lightweight aggregates in the concrete matrix and provide an alternative to obtaining the adequate strength level for the foam concrete. The results of the test showed that the synthetic foam agents were able to act properly as replacements for the lightweight aggregates.
        2.
        2017.04 서비스 종료(열람 제한)
        This study was conducted examine the workability of LEFC in relation to unit quantity of water and fiber addition. The LEFC should secure low weight and good flow by mixing light weight aggregate because the fresh concrete should cured so that gaps do not form between the acrlyic wedges and the concrete with the fresh. The slump tests revealed that fresh concrete with 180 units of water and 0.1% fiber content and fresh concrete with 190 units of water and 0.1%, 0.2% fiber content respectively had excellent workability.
        3.
        2017.01 KCI 등재 서비스 종료(열람 제한)
        This study was conducted to examine the workability of LEFC in relation to the types and the mix ratio of different foaming agents. The foam agents act as lightweight aggregates in the concrete matrix and provide an alternative to obtaining the adequate strength level for the foam concrete. The results of the test showed that the synthetic foam agents were able to act properly as replacements for the lightweight aggregates.
        4.
        2017.01 KCI 등재 서비스 종료(열람 제한)
        This study was conducted examine the workability of LEFC in relation to unit quantity of water and fiber addition. The LEFC should secure low weight and good flow by mixing light weight aggregate because the fresh concrete should cured so that gaps do not form between the acrlyic wedges and the concrete with the fresh. The slump tests revealed that fresh concrete with 180 units of water and 0.1% fiber content and fresh concrete with 190 units of water and 0.1%, 0.2% fiber content respectively had excellent workability.