검색결과

검색조건
좁혀보기
검색필터
결과 내 재검색

간행물

    분야

      발행연도

      -

        검색결과 1

        1.
        2011.08 KCI 등재 구독 인증기관 무료, 개인회원 유료
        Inkjet printing was successfully done using Cu nano powder ink after these Cu nano powders were dry-coated with 1-octanethiol for oxidation prevention. 1-octanethiol, which is Self-Assembled Multi-layers (SAMs), was coated approximately 10-nm thick on the surface of Cu nano powders. 1-Octanol, which has the same chain length as that for 1-octanethiol, was used as a solvent to make the ink for inkjet printing. As a result, the fabricated ink was dispersed for about 4 weeks, and after printing and heat treatment at for 4 hours, the resistivity for the printed pattern was measured to be .
        4,000원