        1.
        2006.09 구독 인증기관·개인회원 무료
        The electrophoretic deposition process of Ni nano-particles was employed for self-repairing of heat exchanger tubes. For electrophoretic deposition of Ni nano-particles on pitted Ni alloy specimen, a constant electric field of 100 V was applied to the specimen for 180 s in Ni-dispersed solution. It was found that as electrophoretic deposition proceeded, the size of the pit remarkably decreased due to the agglomeration of Ni nano-particles at the pit. This strongly suggests that the electrophoretic mobility of the charged particles is larger for the pit with a higher current value rather than outer surfaces with a lower current value.