        1.
        2006.04 구독 인증기관·개인회원 무료
        A QM-ISP-4 Planetary Mill was employed to activate mechanically the mixtures of anatase and corundum at room temperature for different times. The milled powder mixtures were then sintered at for 1 h. The XRD results showed that the milled powder mixtures were completely transformed into after sintering, except the mixtures milled for 5 and 10 hours. The SEM observations showed the typical morphology of rod-like vary in the range: widths from 0.6 to , and lengths from 3.0 to . The rod-like formation was attributed to the positive effects caused by the mechanical activation.