        Biomimetic apatite deposition behaviors on Zr-1Nb and Ti-6Al-4V plate with various surface conditions were examined. Both alloys were polished with abrasive papers to have different roughness and some of them were treated in NaOH before exposition in simulated body fluid. NaOH treatment was found to enhance the deposition rate of apatite on Ti-6Al-4V significantly. On the other hand, the deposition rate of Zr-1Nb was not influenced by NaOH treatment. Without NaOH treatment, the polished Zr-1Nb with abrasive paper was found to induce more apatite nucleation than the polished Zr-6Al-4V.