Wet pavement friction decreases due to the increase in water film thickness (WFT), leading to a significant increase in vehicle crashes occurrences. The British Pendulum Test described in ASTM E303-93 is one of the methods used to measure pavement friction in wet conditions for the input of geometric design and pavement management systems. The British Pendulum Number (BPN) in wet conditions varies with WFT. Following ASTM E303-93 standard procedures, water film thickness was simulated by spraying water on the pavement surface. However, the measurement of BPN did not include specific information about the thickness of the water film present during testing. To address these issues, WFTs and BPNs were measured using artificial rainfall generated by a rainfall simulator across various intensities, drainage lengths, pavement slopes, and pavement surfaces. This study aims to investigate the influence of water film thickness on BPN for wet pavement friction and provide the WFT corresponding to each BPN measurement for different surface types. BPNs of three test slabs, including a smooth surface and tined surfaces with 16 mm and 25 mm spacing, were measured under wet conditions by spraying water, and by creating water film thicknesses using a rainfall simulator. This study demonstrates that the BPNs of non-tined surfaces and longitudinally and transversely tined surfaces with 25mm spacing exhibit a significant decrease with increasing water film thickness, while those with 16mm spacing show a slight decrease. These findings can be attributed to the lower friction observed in both non-tined and longitudinally tined pavements, in contrast to surfaces with transverse tinning.
PURPOSES : The skid resistance between tires and the pavement surface is an important factor that directly affects driving safety and must be considered when evaluating the road performance. In especially wet conditions, the skid resistance of the pavement surface decreases considerably, increasing the risk of accidents. Moreover, poor drainage can lead to hydroplaning. This study aimed to develop a prediction equation for the roughness coefficient—that is, an index of frictional resistance at the interface of the water flow and surface material—to estimate the thickness of the water film in advance to prevent human and material damage. METHODS : The roughness coefficient can be changed depending on the surface material and can be calculated using Manning's theory. Here, the water level (h), which is included in the cross-sectional area and wetted perimeter calculations, can be used to calculate the roughness coefficient by using the water film thickness measurements generated after simulating specific rainfall conditions. In this study, the pavement slope, drainage path length, and mean texture depth for each concrete surface type (non-tined, and tined surfaces with 25-mm and 16-mm spacings) were used as variables. A water film thickness scale was manufactured and used to measure the water film thickness by placing it vertically on top of the pavement surface along the length of the scale protrusion. Based on the measured water film thickness, the roughness coefficient could be back-calculated by applying Manning's formula. A regression analysis was then performed to develop a prediction equation for the roughness coefficient based on the water film thickness data using the water film thickness, mean texture depth, pavement slope, and drainage path length as independent variables. RESULTS : To calculate the roughness coefficient, the results of the water film thickness measurements using rainfall simulations demonstrated that the water film thickness increased as the rainfall intensity increased under N/T, T25, and T16 conditions. Moreover, the water film thickness decreased owing to the linear increase in drainage capacity as the mean texture depth and pavement slope increased, and the shorter the drainage path length, the faster the drainage, resulting in a low water film thickness. Based on the measured water film thickness data, the roughness coefficient was calculated, and it was evident that the roughness coefficient decreased as the rainfall intensity increased. Moreover, the higher the pavement slope and the shorter the drainage path length, the faster the drainage reduced the water film thickness and increased the roughness coefficient (which is an indicator of the friction resistance). It was also evident that as the mean texture depth increased, the drainage capacity increased, which also reduced the roughness coefficient. CONCLUSIONS : As the roughness coefficient of the concrete road surface changes based on the environmental factors, road geometry, and pavement surface characteristics, we developed a prediction equation for the concrete pavement roughness coefficient that considered these factors. To validate the proposed prediction equation, a sensitivity analysis was conducted using the water film thickness prediction equation from previous studies. Existing models have limitations on the impact of the pavement type and rainfall intensity and can be biased toward underestimation; in contrast, the proposed model demonstrated a high correlation between the calculated and measured values. The water film thickness was calculated based on the road design standards in Korea—in the order of normal, caution, and danger scenarios—by using the proposed concrete pavement roughness coefficient prediction model under rainy weather conditions. Specifically, because the normal and caution stages occur before the manifestation of hydroplaning, it should be possible to prevent damage before it leads to the danger stage if it is predicted and managed in advance.
Since the decrease of skid resistance of the road surface due to the effects of hydroplaning increases the ratio of vehicle crashes significantly, it is important to predict water film thickness (WFT). Tined is one of the widely used textures for concrete pavements. Since previous WFT models have been developed based on the asphalt pavement texture and broom concrete, it may not give reliable predictions for Water film thickness for tinned concrete. Furthermore, surface flow on tined texture may show hydraulically different characteristics due to the geometric characteristics of tined texture. This study aims to propose a reliable water film thickness prediction model for tined concrete. Three test slabs including a smooth surface, a tined surface with 16mm spacing, and a tined surface with 25mm spacing were prepared. WFTs of the test slab were measured for various conditions such as pavement slope (0-10%), rainfall intensity (0-130mm/h), and drainage path length (0-5m). A statistical model was proposed to predict water film thickness (WFT) as a function of pavement slope, rainfall intensity, drainage path length, and mean texture depth. This model exhibits strong agreement with the experimental test results. The GWNU prediction model consistently provides reliable predictions with the actual WFT for tined concrete pavement. Conversely, the previous equation consistently underestimated the water film thickness, notably on tined surfaces with 16 mm and 25 mm spacing, due to the occurrence of viscous flow along the tined lines.
여름철은 타 계절에 비해 장마와 불안정한 대기 등으로 인하여 빗길 교통사고의 위험성이 크게 증대될 수 있으며, 최근 5년 (2018~2022)간 여름철 빗길 교통사고는 전체 빗길 교통사고의 39%를 차지할 정도로 높은 수준이다. 이러한 빗길 운전은 노면의 배수 불량 및 미끄럼 저항 감소 등으로 인하여 수막현상을 발생시키게 된다. 이에 본 연구에서는 우천 시 도로의 안전성 강화 및 사고 위 험을 최소화하기 위한 요소인 수막두께를 산정하기 위하여 Manning의 평균 유속식을 기반으로 콘크리트 노면의 조도계수 예측 모델을 개발하는 것을 목표로 하였다. 조도계수의 영향인자를 고려하기 위하여 실외 강우 모의 장비를 이용하여 콘크리트를 타설한 뒤 실험 인자로 포장 경사, 배수거리, 강우강도, 노면 조직 특성을 고려하였으며, 이 중 노면 조직 특성은 타이닝 처리를 하지 않은 구간만 고 려한 타 연구의 기존 예측 모델 단점을 보완하기 위하여 16, 25mm 간격의 타이닝 표면 처리한 구간을 추가로 고려하였다. 수막두께 측정은 측정 범위 0.3~5mm의 수막두께 측정 게이지를 제작하여 강우가 모사된 조건에서 배수 거리 1~5m 이내 지점의 노면 조직 상 단과 수면이 접하는 수직 높이를 총 3회 측정하여 평균값을 사용하였다. 실측된 수막두께 데이터베이스를 기반으로 Manning 공식을 이용하여 조도계수를 역산한 결과, 강우강도가 증가함에 따라 조도계수는 감소하였으며, 이는 강우의 증가로 인해 물의 흐름과 콘크리 트 노면 사이의 마찰 저항 감소에 기인한 것으로 판단되었다. 또한 포장 경사가 높고 배수 거리가 짧을수록 배수성이 증가하여 마찰 저항의 지표인 조도계수가 증가하는 것으로 확인되었다. 평균 조직 깊이에 따른 조도계수 영향의 경우, 평균 조직 깊이가 증가할수록 콘크리트 표면에 노출되는 표면적이 증가하여 수막두께가 얕게 생성되고, 얕은 수심으로 인해 물의 흐름 저항이 감소하여 조도계수는 감소하는 것으로 산정되었다. 이후 135개의 데이터를 종합하여 조도계수를 종속변수로 하고 강우강도, 포장경사, 배수거리, 평균 조직 깊이, 수막두께를 독립변수로 하는 회귀분석을 수행하여 조도계수 산정식을 개발하였다.
Load carrying capacity(LCC) can be reduced from its design value as a result of film thickness change when a journal is misaligned and some part of bearing is unintentionally translated. In this study, the numerical solution of the incompressible Reynolds equation was obtained by using the finite difference method and mass conservation algorithm (JFO boundary condition) with periodic pressure distribution in circumferential direction to analyze the change of LCC due to journal misalignment and step change of film thickness in axial direction for a journal bearing of vertical pumps. Smallest LCC in each eccentricity ratio is obtained as two angular positions are changed – an angular position where misalignment occurs, and another angular position where the axial step takes place while the degree of misalignment is fixed at 90%. Compared with the reaction force of plain journal bearing, the LCC reduced as much as 26.7% due to geometric effects of journal bearing at the eccentricity ratio of 0.9, while the step height is no higher than 0.1 times of bearing clearance.