간행물

한국분말야금학회 학술대회논문집

권호리스트/논문검색
이 간행물 논문 검색

권호

한국분말야금학회 2004년도 학술대회논문집 (2004년 6월) 122

101.
2004.06 구독 인증기관·개인회원 무료
Using the high-frequency induction heated combustion method, the simultaneous synthesis and densification of (x=0, 10, 20, 30) composites was accomplished using elemental powders of W, Si and C. A complete synthesis and densification of the materials was achieved in one step within a duration of 2 min. The relative density of the composite was up to 97% for the applied pressure of 60MPa and the induced current. The average grain size of are 6.9, 6.1, and , respectively. The hardness and the fracture toughness increases with increasing SiC content. The maximum values for the hardness and fracture toughness are .
103.
2004.06 구독 인증기관·개인회원 무료
(1) Using high-frequency induction heating sintering and spark plasma sintering method, the densification of WC-Ni hard materials was accomplished using ultra fine power of Ni and WC. (2) Nearly fully dense WC-Ni could be obtained within 1 min. (3) Relative density and mechanical properties of WC-Ni obtained by HFIHS were high than those obtained by SPS. And WC grain size made by HFIHS was smaller than that made by SPS. (4) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by HFIHS were , respectively for 60MPa and an induced current for 90% output of total capacity, 15KW. (5) The fracture toughness and hardness values of WC-8Ni, WC-10Ni, and WC-12Ni made by SPS were , respectively for 60MPa and the electric current of 2500 A
6 7