검색결과

검색조건
좁혀보기
검색필터
결과 내 재검색

간행물

    분야

      발행연도

      -

        검색결과 77

        61.
        1999.06 KCI 등재 구독 인증기관 무료, 개인회원 유료
        In order to introduce the touch to engineering and industries, it must be preceded to dstablish a quantitative barometer of the feeling. for this purpose, we developed a tactile measuring system to measure physical properties of texture, such as surface roughness, friction coefficient and compliance. The tactile measuring system uses a LASER type displacement sensor, which is a non-contacting system, in measuring the surface roughness. By considering that human tactile system is a contacting mechanism, this non-contacting method needs to be modified. As a precedent research of that, we compared the contacting and non-contacting method in this paper. Surface roughness of ten cloths were measured by using the measuring system, then compared to the test results using the Kawabata evaluation system(KES), which uses a contacting method in measuring the surface roughness.
        4,000원
        62.
        1999.02 KCI 등재 구독 인증기관 무료, 개인회원 유료
        In this paper, the wind tunnel test was carried to investigate the behavior of buffer layer in turbulent boundary layer with variation of surface temperature and roughness. The results were as follows; 1. The velocity in turbulent boundary layer was increased when the roughness height within viscous sublayer thickness was increased. 2. When the surface temperature was increased, the density of air was decreased and the velocity in turbulent boundary layer was increased. Thus, the thickness of turbulent boundary layer was decreased. 3. When the roughness height and surface temperature was increased simultaneously, the thickness of turbulent boundary layer was decreased. 4. The decrement of the thickness of turbulent boundary layer was more effected by the increment of the roughness height rather than the increment of surface temperature. 5. In this study, it was found that the condition of the highest velocity n turbulent boundary layer was the temperature 333K and roughness #100.
        4,000원
        63.
        1998.01 KCI 등재 SCOPUS 구독 인증기관 무료, 개인회원 유료
        RTCVD법으로 증착된 다결정 Si1-xGex박막에서 Ge조성 증가에 따른 결정립크기변화가 표면거칠기 및 cluster크기에 미치는 영향에 대해 알아본결과, Ge조성 증가에 따라 결정립크기가 증가했으며 증가된 결정립에 의해 Cluster 크기와 표면거칠기값(RMS)들이 증가함을 알 수 있었다. 또한 증착된 다결정 Si1-xGex박막을 RF power와 온도변화에 따라 Ar/H2플라즈마를 이용한 수소화처리를 행하여, 수소화 효과와 표면거칠기값 그리고 비저항값 변화에 대해 조사하였다. 수소화처리 후 cluster크기와 표면거칠기값은 기판온도와 RF power 증가에따라 감소함을 알 수 있었으며 특히 기판온도 300˚C에서는 비저항값이 상당히 증가하였다.
        4,000원
        64.
        1997.11 KCI 등재 SCOPUS 구독 인증기관 무료, 개인회원 유료
        LED와 LD의 수명과 효율은 결정에 존재하는 결함의 밀도에 반비례하며, 이러한 결함의 밀도는 적당한 기판을 사용하거나, 기판의 표면을 적절하게 제어함으로써 줄일 수 있다. GaN성장시 원자 단위의 매끄러운 표면은 완충충 성장이나 질화처리를 함으로써 얻어질 수 있다. 이렇게 얻어진 원자 단위의 매끄러운 표면에 의해 기판과 박막상이의 계면 자유에너지가 감소하기 때문에 2D성장이 촉진된다. 사파이어(AI2O3(0001))기판을 사용한 GaN 왕충충성장과 진화처리에 대한 최적조건은 AFM(Atomic Force Microscope)측정 결과에 의해 결정되었다. AFM에 의해 얻어진 표면 평활도의 개념은 사파이어 기판을 사용한 GaN박막성장의 최적조건을 결정하는 데 있어서 높은 신뢰도를 가질 수 있다.
        4,000원
        65.
        1994.05 KCI 등재 구독 인증기관 무료, 개인회원 유료
        There has been studied a lot of two dimensional hydrofoil sections for the boundary layers. This paper suggests that the plaiable roughness effects on boundary layer transition region of suction side for NACA 4412 hydrofoil sections provided by auxieiary shape factor and lag-entrainment effects. These results show that the laminar sepration. Transition and end of transition of the boundary layer due to pitting roughness effects, to the foil Reynold's number as well as to the angle of attack were delayed a little. And comparisons with valuable the other calculations and measurements show qualitative agreements.
        4,000원
        66.
        2022.09 KCI 등재 서비스 종료(열람 제한)
        지표에 노출된 암석은 지속적으로 풍화를 받게 되고 이러한 영향으로 암석의 공학적 안정성이 약해 지게 된다. 특히 풍화가 진행되면서 암석의 표면은 풍화에 의해서 변화를 일으키고 이러한 표면 변화는 암석 으로 구성된 지반의 공학적 안전성에 영향을 미치게 된다. 또한, 풍화를 받은 암석에서 생성되는 화학종은 주 변환경에 직접적인 영향을 미치거나 구조물에 영향을 미치게 된다. 광산지역과 같이 암석이 노출된 지역에서 는 풍화에 의해 생성된 화학종이 주변 자연환경에 심각한 영향을 미치기도 한다. 본 연구에서는 이러한 관점 에서 동결/융해 실험을 활용한 풍화가속 실험을 이미 풍화를 받은 암석과 신선한 암석을 대상으로 실시하고 각 암석의 표면 변화를 다초점 레이저 현미경으로 관찰하고 IC/ICP-MS를 활용하여 화학종 생성에 대한 분 석을 실시하였다. 풍화가 진행됨에 따라 표면의 거칠기는 완화되는 것을 확인하였고 주변환경에 영향을 미칠 수 있는 화학종은 풍화를 받는동안 양이 증가하는 것을 확인하였다. 본 연구 결과는 암석이 노출된 지역에서 의 공학적/환경학적 안전성을 평가하는 기초 자료로 활용될 수 있을 것이다.
        67.
        2018.05 KCI 등재 서비스 종료(열람 제한)
        본 연구에서는 동결융해 작용을 받는 콘크리트의 내구성을 현장에서 평가하기 위한 일환으로 표면 거칠기 값과 이미지 분석을 대 상으로 상대동탄성계수와의 관계를 분석하였다. 배합은 물-시멘트비에 따라 40%, 50%, 60% 및 70% 총 4배합으로 수행하였으며 동해를 조기에 발현시키기 위하여 AE제를 사용하지 않았다. 실험은 물-시멘트비에 따라 상대동탄성계수 및 압축강도 등의 기본 물성 시험과 표면 거칠기 측정, 화상 이미지 및 SEM 이미지 분석을 수행하였다. 표면 거칠기 시험 결과 물-시멘트비에 상관없이 전반적으로 싸이클이 증가함에 따라 표면거칠기 값이 증가하는 경향을 보였으며 상대적으로 조밀한 40% 및 50%의 경우 상대동탄성계수가 60% 이하인 시점까지 서서히 증가하는 경향을 보였으나, 60% 및 70%의 경우 파괴 시점에서만 표면 거칠기 값이 증가하였다. 또한, 표면부 화상 이미지 분석에서도 물-시멘트비 40% 및 50%의 경우 동결융해 싸이클이 진행되는 과정에서 표면부터 서서히 열화가 진행되는 과정을 확인할 수 있었으나 60% 및 70%의 경우 표면 부의 변화가 미미하다 파괴 시점에서 균열 등의 손상을 확인할 수 있었다. 따라서, 상대적으로 수밀하지 않은 시험체의 경우 화상 이미지나 표면 거칠기 등의 인자로 동결융해의 열화 정도를 판별하기에는 일부 제한이 있을 것으로 판단되며 상대적으로 수밀한 W/C 40% 및 50%의 경우 표면 거칠기 및 표면부 화상 이미지로 동해의 열화 진행 정도를 판단할 수 있었으며 향후 현장에서 표면 거칠기 및 이미지 분석을 적용할 수 있을 것으로 판단된다.
        68.
        2017.04 서비스 종료(열람 제한)
        In this study, To evaluate the durability of concrete by freezing-thawing, relative dynamic modulus of elasticity and surface roughness were measured. The results showed that the surface roughness can be used to understand the damage tendency of freezing-thawing and the durability of concrete.
        69.
        2017.01 KCI 등재 서비스 종료(열람 제한)
        In this study, To evaluate the durability of concrete by freezing-thawing, relative dynamic modulus of elasticity and surface roughness were measured. The results showed that the surface roughness can be used to understand the damage tendency of freezing-thawing and the durability of concrete.
        70.
        2011.01 KCI 등재 서비스 종료(열람 제한)
        Physically-based resampling scheme for roughness coefficient of surface runoff considering the spatial landuse distribution was suggested for the purpose of effective operational application of recent grid-based distributed rainfall runoff model. Generally grid scale(mother scale) of hydrologic modeling can be greater than the scale (child scale) of original GIS thematic digital map when the objective basin is wide or topographically simple, so the modeler uses large grid scale. The resampled roughness coefficient was estimated and compared using 3 different schemes of Predominant, Composite and Mosaic approaches and total runoff volume and peak streamflow were computed through distributed rainfall-runoff model. For quantitative assessment of biases between computational simulation and observation, runoff responses for the roughness estimated using the 3 different schemes were evaluated using MAPE(Mean Areal Percentage Error), RMSE(Root-Mean Squared Error), and COE(Coefficient of Efficiency). As a result, in the case of 500m scale Mosaic resampling for the natural and urban basin, the distribution of surface runoff roughness coefficient shows biggest difference from that of original scale but surface runoff simulation shows smallest, especially in peakflow rather than total runoff volume.
        71.
        2010.08 KCI 등재 서비스 종료(열람 제한)
        해양의 다양한 환경에 노출된 선체 표면의 거칠기를 일반화 하여 모델 실험을 PIV기법을 적용하여 회류수조에서 수행하였다. 모델의 유동방향 표면 거칠기의 폭에 기초하여 본 연구에 적용된 레이놀즈수 Re=1.0×103에서 유동가시화, 시간평균 속도장 및 와도장을 상호 평가를 통하여 유동특성을 조사하였다. 와의 생성과 소멸 메커니즘을 통해 와류의 중심은 표면 거칠기 높이의 0.5H로 나타났다. 또한 거칠기 계수가 증가함에 따라 와의 크기와 비례하고, 와의 생성위치도 상부와 전방으로 이동하였다.
        72.
        2010.01 KCI 등재 서비스 종료(열람 제한)
        철근부식에 의해 발생된 녹은 철근 주위의 콘크리트에 팽창압력을 발생시켜 콘크리트의 균열유발, 피복콘크리트의 박리나 탈락, 철근의 단면적 감소들을 야기 시킨다. 또한 철근콘크리트 구조물 내에 매입된 철근의 부식은 철근과 콘크리트의 일체 거동을 저하시킴으로써 구조물이 외력에 견딜 수 있는 구조성능의 감소를 초래한다. 본 논문에서는 3차원 스캐너를 이용하여 철근이 부식됨에 따른 철근의 표면적을 측정하여 부식률과 표면 거칠기와의 관계를 파악하였다. 철근부식률 1~2%의 경우에서는 철근 표면적이 증가하는 것으로 나타났다. 이는 동일 범위내에서 철근의 부착강도가 증가한 기존의 실험결과와 매우 유사한 결과를 나타낸다. 철근부식률 2% 이상에서는 오히려 표면적이 감소하였으며, 이는 단면적 손실로 인한 기존 부착강도 실험과 부합되는 결과를 나타냈다
        76.
        1999.12 KCI 등재 서비스 종료(열람 제한)
        Effects of surface conditions (temperature and roughness) of test specimens, when measuring emissive power of far-infrared ray, have been investigated using FT-IR spectrometer. Element metal zinc (Zn) was selected in this study as representative specimen of materials consisting of simple element. The zinc specimens were heated to four temperatures, i.e., 333K, 353K, .373K, and also their surface was finished with SiC abrasive papers of 100, 220, 360, 400, 600, 800, and 1000 mesh in size. The results shows that the emissive power (W/㎡) of the far-infrared ray increases with temperature for a given roughness and its relationship may be expressed by the following equations: Yη=1.0=0.142.T-0.937 for η=1.0, and Yη=10=0.016.T-1.286 for η=10. The emissive power is also known to increase with surface roughness for a given temperature. Their relationship can be represented by the following equations: YT=313K=0.234.ln(η)+3.53, at 313K, YT=353K=0.234.ln(η)+4.02 at 353K and YT=393K=0.243.ln(η)+4.62 at 393K.
        77.
        1997.12 KCI 등재 서비스 종료(열람 제한)
        This paper discussed effect of the surface roughness and the hydrophobicity of support material on the microbial attachment in a rotating biological contactor. The hydrophobicity of each support material was determined by the measurement of contact angle of water and the surface roughness was measured by the surface roughness instrument. Microorganisms have well attached on the surface of more hydrophilic support material like Nylon6 than that of the hydrophobic support material like PE. When the relatively hydrophilic surface was roughen, the microbial attachment was increased but when the relatively hydrophobic surface was roughen, the attachment was slightly increased because the hydrophobicity of support material was increased by roughening the hydrophobic surface. Although both variables, the surface hydrophobicity and the surface roughness, have influenced the microbial attachment, the influence of the surface roughness overruled that of the surface hydrophobicity. Support material whose surfaces were roughened about l㎛, 6㎛ and 11㎛ were allowed for attached 3, 7 and 24hr, but the differences of maximum and minimum attachment of each material gave nearly constant values and similar trend with time.
        1 2 3 4