A novel production method for porous metal components has been developed by applying powder space holder (PSH) method to metal powder injection molding (MIM) process. The PSH-MIM method has an industrial competitive advantage that is capable of net-shape manufacturing the micro-sized porous metal products with complicated shapes and controlled porosity and pore size. In this study, the small impeller with homogeneous micro-porous structure was manufactured by the PSH-MIM method. The effects of combinations in size and fraction of PMMA particle on dimensional tolerance and variation of sintered porous specimens were investigated. It was concluded that the PSH-MIM method could manufacture commercially microporous metal components with high dimensional accuracy.
In recent years, micro powder injection molding is being explored as an economical fabrication method for microcomponents in microsystems technology (MST). Technical and economic comparison was performed for processes. Molding experiment and simulation during the filling process were performed to evaluate several different geometries and processing conditions. The influence of material parameters and process conditions on mold filling were examined as a function of features size using microchannels as an example. It was found that the heat conductivity and viscosity of feedstock, geometry and mold temperature were the most critical parameters for complete filling of micro features.
Small powder size is very useful in achieving detailed structures. STS 316 nanopowders with an average diameter of 100 nm and were utilized to produce feedstock. The mixing behavior of the feedstock indicated that the nanoparticle feedstock produced the highest mixing torque at various powder loading compared to the micropowder feedstock. The nanoparticles feedstocks showed that elastic properties are dominant in flow behavior and high viscosity. Conversely the micropowders feedstocks, viscous properties are dominant in flow behavior and less viscosity, nanopowders feedstock perform lower flow activation energy than feedstock with bigger particles.
통상적인 금속분말의 성형은 분말야금 공정으로 이루어지기 때문에 복잡한 형상의 부품을 구현하는 데는 제약이 있다. 하지만, 1970년대 후반 이래 새로운 금속분말의 성형기술로 크게 각광을 받으며 연구되고 있는 금속분말사출성형(Metal Powder Injection Molding, MIM) 기술을 이용하면 다양한 형태의 부품을 성형할 수 있다 최근에는 이러한 MIM 기술을 이용하여 다양한 산업분야에 응용될 수 있는 마이크로 부품을 제조하고자 하는 연구개발
The production of micro components is one of the leading technologies in the fields of information and communiation, medical and biotechnology, and micro sensor and micro actuator system. Microfabrication (micromachining) techniques such as X-ray lithography, electroforming, micromolding and excimer laser ablation are used for the production of micro components out of silicon, polymer and a limited number of pure metals or binary alloys. However, since the first development of microfabrication technologies there have been demands for the cost-effective replication in large scale series as well as the extended range of available material. One such promising process is micro powder injection molding (PIM), which inherits the advantages of the conventional PIM technology, such as low production cost, shape complexity, applicability to many materials, applicability to many materials, and good tolerance. This paper reports on a fundamental investigation of the application of W-Cu powder to micro metal injection molding (MIM), especially in view of achieving a good filling and a safe removal of a micro mold conducted in the experiment. It is absolutely legitimate and meaningful, at the present state of the technique, to continue developing the micro MIM towards production processes for micro components.