한국분말야금학회 2006년도 춘계학술대회논문집 (2006년 4월) 443

281.
2006.04 구독 인증기관·개인회원 무료
Pure and stable YAG powders were synthesized by a PVA (polyvinyl alcohol) polymer solution technique. PVA was used as an organic carrier for the precursor ceramic gel. The precursor gels were crystallized to YAG at relatively a low temperature of . The synthesized powders, which have nano-sized primary particles, were soft and porous, and the porous powders were ground to sub-micron size by a simple ball milling process. The ball-milled powders were densified to 94% relative density at for 1h. In this study, the characteristics of the synthesized YAG powders were examined.
282.
2006.04 구독 인증기관·개인회원 무료
Several titanate powders (, etc.) were synthesized by an ethylene glycol solution route. Titanium isopropoxide and nitrate salts were dissolved in stoichiometric proportions in liquid-type ethylene glycol without any precipitation. The parent precursor sols were dried to porous gels, and then the gels were calcined and crystallized. All synthesized titanate powders had stable crystallization behavior at low temperature and high specific surface area after a simple ball-milling process. A three-component PZT powder was also synthesized successfully by the ethylene glycol method. In this study, the characteristics of the multi-component titanate powders by the ethylene glycol method are examined.
283.
2006.04 구독 인증기관·개인회원 무료
Vacuum carbonization of nanometer tungsten powder was investigated in a simple designed apparatus. An X-Y recorder was used to plot differential thermal analysis (DTA) curves to determine starting temperature of carbonization of four samples with different specific surface area. The product was detected by X-ray Diffraction (XRD) and small angle X-ray scattering (SAXS). The results show that finer tungsten powder has lower starting temperature of carbonization. Tungsten powder, which BET surface area is , is completely carbonized to tungsten carbide at , although the starting temperature is . Particle grows sharply before carbonization.
284.
2006.04 구독 인증기관·개인회원 무료
Flying trajectories of fine particles within a size range of were studied during centrifugal atomizing processes. A FORTRAN program was written by using increment method. Calculation results revealed that the drag force might reach very high value of 522-7800 g for fine powder of . Flying distance in horizontal direction could be shortened if the particles fly obliquely due to the huge drug force. On the other hand, very fine powder could be projected to far distances when the atmosphere flow velocity is much stronger. Fortunately such particles could be contracted within a cylinder closed to the atomizer when the atmosphere flow was weaken or retained in a limited diameter.
285.
2006.04 구독 인증기관·개인회원 무료
Magnetic oxide-coated iron nanoparticles with the mean size ranging from 6 to 75 nm were synthesized by aerosol method using iron carbonyl as a precursor under the flowing inert gas atmosphere. Oxide shells were formed by passivation of asprepared iron particles. The influence of experimental parameters on the nanoparticles' microstructure, phase composition and growth behavior as well as magnetic properties were investigated and discussed in this study.
288.
2006.04 구독 인증기관·개인회원 무료
This paper described the preparation method for composing high-grade synthetic diamond by water atomizing using FeNi30 powder catalyst. The objective of this article is about powder making process using super high water atomizing in the atmosphere of inert gas, and then corroded the powder with a corrosion inhibitor. Finally, FeNi30 catalyst powder with lower oxygen content and good sphericity is produced. The experiment of making diamonds by using cubic press and the performance of the diamonds are also discussed.
289.
2006.04 구독 인증기관·개인회원 무료
The influence of Hi-flux powders characteristics on the performance of magnetic powder cores was studied. It was found that different cooling rate and nozzle configuration could change the shape and microstructure of powders. Smooth surface and spherical shape of powders were beneficial to improve DC bias performance and reduce core losses of magnetic powder core.
293.
2006.04 구독 인증기관·개인회원 무료
We have demonstrated that textured nanocomposites can be fabricated by slip casting followed by partial oxidation. reaction sintering of mixed suspensions of and SiC powders in a high magnetic field. The sintered density was changed by the degree of oxidation at 1200C and 1300C. The degree of orientation of alumina in the nanocomposite was examined on the basis of the X-ray diffraction patterns and scanning electron micrographs. It is confirmed that aluminaoriented nanocomposites were fabricated. The three-point bending strength at room temperature was observed for the nanocomposites.
295.
2006.04 구독 인증기관·개인회원 무료
N-type solid solutions doped with 1 was prepared by melt spinning, crushing and vacuum sintering processes. Microstructure, bending strength and thermoelectric property were investigated as a function of the doping quantity from 0.03wt.% to 0.10wt.% and sintering temperature from to , and finally compared with those of conventionally fabricated alloys. The alloy showed a good structural homogeneity as well as bending strength of . The highest thermoelectric figure of merit was obtained by doping 0.03wt.% and sintering at .
297.
2006.04 구독 인증기관·개인회원 무료
Monodispersed and nano-sized Ni powders were synthesized from aqueous nickel sulfate hexahydrate inside nonionic polymer network by using wet chemical reduction process. The sucrose was used as a nonionic polymer network source. The effect of reaction conditions such as the amount of sucrose and a various reaction temperature, nickel sulfate hexahydrate molarity. The influence of a nonionic polymer network on the particle size of the prepared Ni powders was characterized by means of X-ray diffraction (XRD), scanning electron microscopy (SEM), and particle size analysis (PSA). The results showed that the obtained Ni powders were strong by dependent of the reaction conditions. In particular, the Ni powders prepared inside a nonionic polymer network had smooth spherical shape and narrow particle size distribution.
298.
2006.04 구독 인증기관·개인회원 무료
Monodispersed and nano-sized Cu powders were synthesized from copper sulfate pentahydrate inside a nonionic polymer matrix by using wet chemical reduction process. The sucrose was used as a nonionic polymer network source. The influences of a nonionic polymer matrix on the particle size of the prepared Cu powders were characterized by means of X-ray diffraction), scanning electron microscopy), and particle size analysis). The smallen Cu powders with size of approximately 100 nm was obtained with adding of 0.04M sucrose at reaction temperature of . The particle size of the Cu powders prepared by the reduction inside polymer network was strongly dependent of the sucrose content and reaction temperature.
299.
2006.04 구독 인증기관·개인회원 무료
The anatase particle was facetted at the free surface and a neck formation between the anatase particles prior to the phase transformation occured. This resulted in the severe lattice distortion at the region of the interface near the neck and this can act as the nucleation sites for the phase transformation. The grain growth of rutile particles after the phase transformation grew very fast by the sweeping phenomena of grain boundary. Therfore, It leaded to the microstructure without the rutile phase located in anatase particle.